Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.138 GPa | 310.1 ksi | ASTM D638 |
Ineos Nova 5120 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |
|||
Modulus of Elasticity | 2.138 GPa | 310.1 ksi | ASTM D638 |
Ineos Nova 5124 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |