Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.220 GPa | 31.9 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PE 1270
(discontinued **) PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 12.. |
|||
Modulus of Elasticity | 0.220 GPa | 31.9 ksi | Secant; ASTM D638 |
Huntsman PE 1402 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Modulus of Elasticity | 0.220 - 11.05 GPa @Temperature -100 - 250 °C |
31.9 - 1603 ksi @Temperature -148 - 482 °F |
Average value: 5.50 GPa Grade Count:19 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Modulus of Elasticity | 0.220 - 11.5 GPa @Temperature 60.0 - 150 °C |
31.9 - 1670 ksi @Temperature 140 - 302 °F |
Average value: 5.24 GPa Grade Count:14 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Modulus of Elasticity | 0.220 GPa | 31.9 ksi | ISO 1184-1983E |
LyondellBasell Montell 8340 Polybutene-1 Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements.. |