Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 200 GPa | 29000 ksi | RT |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | RT |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | RT |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
Latrobe LSSâ„¢ Chipper Knife Tool Steel (ASTM A8 Mod.) TLS Chipper Knife tool steel is an air-hardening, 8% chromium tool steel which exhibits very good wear resistance and toughness. TLS Chipper Knife exhibits wear resistance which is better than that.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 100 °C |
29000 ksi @Temperature 212 °F |
|
Haynes 556® alloy, bar, after 1000 hours at 870°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
HP Alloys Alloy 718, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | (hardened to 46 HRC) |
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel Hot Rolled Carbon Steel, Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Dent Resistant (DR 180) Compared to DS Type B, DR steels have higher initial YS which contributes to increased strength after forming.Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
Carpenter Micro-Melt® 9 Hardened and Tempered Tool Steel Micro-Melt® 9 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with goo.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (FS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 8.5% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | in tension |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 20% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | in tension |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 40% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel Cold Rolled Carbon Steel, Bake Hardenable (BH 180), SAE J2340 Type 180 B Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel Type 1, Grade 40 Cold Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 204°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | in tension |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 0% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | in tension |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC Allegheny Ludlum Type 410HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 204°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |