Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 20.0 - 62.0 GPa | 2900 - 8990 ksi | Average value: 38.2 GPa Grade Count:3 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1-1114 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Indium Corp. Indalloy 149 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | Young's modulus; "ab" direction |
Momentive Performance Materials "PG" Pyrolytic Graphite Pyrolytic Graphite (PG) is a unique form of graphite manufactured by decomposition of a hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is ne.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1/XCF/20 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1-0784 Polyamide 66, with glass fiber and carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | Young's modulus |
Momentive Performance Materials Pyrolytic Graphite (PG) Coating PG is a popular coating for sealing machined graphite hardware which does not require oxidation protection. It is the most anisotropic commercially available material and is therefore useful where .. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
SGL Carbon Group EK 2239 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | |
CeramTec ALUTIT® S Aluminum Titanate (Strength Optimized) ALUTIT®, which is produced in a special reaction-sintering process, consists of high-purity aluminum oxide and titanium oxide. It offers excellent resistance to sudden changes in temperature, good .. |
|||
Modulus of Elasticity | 20.0 GPa @Thickness >=1.50 mm |
2900 ksi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 |
Elektro-Isola Etronit AS Phenolic, Paper Reinforcement, Black, Sheets Description: ESD-protection quality according to SP-method 2472, IEC 61340-5-1 and EN 100015-1. SP ESD Approval Certificate No. 230-01-0137. High mechanical properties at temperatures up to 120°CAp.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | DIN 53 457 |
Albis Plastics Tedur® L 9523 PPS, 60% Glass Fiber/Mineral Extremely Rigid, Excellent Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Insulating Equipment, Reflectors and Fitting.. |
|||
Modulus of Elasticity | 20.0 GPa | 2900 ksi | Y; ASTM D3039 |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |