Polymer Property : Modulus of Elasticity = 26.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.180 - 0.900 GPa

@Temperature 60.0 - 120 °C
26.1 - 131 ksi

@Temperature 140 - 248 °F
Average value: 0.505 GPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Modulus of Elasticity 0.180 GPa
26.1 ksi
MD; ISO R527-1
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene
LDPE 2100TN00: Heavy duty film suitable for application in shrink hoods, industrial sacks, heavy duty carrier bags and liners.Information provided by Iran Petrochemical Commercial Co.
Modulus of Elasticity 0.180 - 0.483 GPa
26.1 - 70.1 ksi
Average value: 0.318 GPa Grade Count:10
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum ..