Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 17.2 - 19.3 GPa | 2500 - 2800 ksi | Average value: 18.4 GPa Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Modulus of Elasticity | 17.2 GPa | 2500 ksi | |
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **) Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun.. |
|||
Modulus of Elasticity | 17.2 GPa | 2500 ksi | |
Corning Vycor® 7930 Porous Glass Open cell porous glass which exhibits excellent moisture absorbing properties ("thirsty"). It is mechanically hard and strong, nondusting, nonflaking, and chemically inert. These properties allow .. |