Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 16.7 GPa | 2420 ksi | ISO 527-1/-2 |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |