Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 15.0 - 18.0 GPa | 2180 - 2610 ksi | Injection and Compression; ISO 527 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Modulus of Elasticity | 15.0 - 18.0 GPa | 2180 - 2610 ksi | Injection and Compression; ISO 527 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Modulus of Elasticity | 15.0 - 18.0 GPa | 2180 - 2610 ksi | Injection and Compression; ISO 527 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Modulus of Elasticity | 15.0 - 18.0 GPa | 2180 - 2610 ksi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Modulus of Elasticity | 15.0 - 18.0 GPa | 2180 - 2610 ksi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
Modulus of Elasticity | 15.0 - 18.0 GPa | 2180 - 2610 ksi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | ASTM D638 |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Modulus of Elasticity | 15.0 - 42.0 GPa @Temperature 60.0 - 150 °C |
2180 - 6090 ksi @Temperature 140 - 302 °F |
Average value: 29.5 GPa Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1105-7506 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1105-8000 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1105-8169 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically .. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 55-7880 PC/ABS Alloy, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 80-7917 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1/CF/20/TF/15 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1-1119-1 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | In Tension |
Cytec Thornel® VCK Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | In Tension |
Cytec Thornel® VCL Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | ASTM D638 |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Modulus of Elasticity | 15.0 GPa | 2180 ksi | |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |