Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.145 GPa | 21.0 ksi | ASTM D638 |
Arkema Group Pebax® 5533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Modulus of Elasticity | 0.145 - 3.30 GPa @Temperature -40.0 - 150 °C |
21.0 - 479 ksi @Temperature -40.0 - 302 °F |
Average value: 0.997 GPa Grade Count:8 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |