Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 140 - 160 GPa | 20300 - 23200 ksi | Youngs Modulus |
MMCC Al/Al2O3 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Modulus of Elasticity | 140 GPa | 20300 ksi | |
CLAL-MSX CUPROROR® TL1 1/4 hard, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Modulus of Elasticity | 140 GPa | 20300 ksi | |
CLAL-MSX CUPROROR® TL2 1/2 hard, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Modulus of Elasticity | 140 GPa | 20300 ksi | |
CLAL-MSX CUPROROR® TL5 Spring, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Modulus of Elasticity | 140 GPa | 20300 ksi | |
CLAL-MSX CUPROROR® TL4 Hard, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 599 °C |
20300 ksi @Temperature 1110 °F |
hardened to 45 HRC |
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 599 °C |
20300 ksi @Temperature 1110 °F |
hardness of 56 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |
|||
Modulus of Elasticity | 140 GPa @Temperature 599 °C |
20300 ksi @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 599 °C |
20300 ksi @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 599 °C |
20300 ksi @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 600 °C |
20300 ksi @Temperature 1110 °F |
|
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |
|||
Modulus of Elasticity | 140 GPa | 20300 ksi | |
ATI Wah Chang Nb/Nb Alloy FS-85 Information provided by ATI Wah Chang |