Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0180 - 0.207 GPa | 2.61 - 30.0 ksi | Average value: 0.0508 GPa Grade Count:9 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Modulus of Elasticity | 0.0180 - 0.0680 GPa | 2.61 - 9.86 ksi | Average value: 0.0313 GPa Grade Count:8 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Modulus of Elasticity | 0.0180 - 0.0800 GPa | 2.61 - 11.6 ksi | Average value: 0.0474 GPa Grade Count:9 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an.. |
|||
Modulus of Elasticity | 0.0180 GPa | 2.61 ksi | ASTM D412 |
KKPC KOSYN KTR 302 Thermoplastic Elastomer (TPE) Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics .. |