Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 119 GPa @Temperature 982 °C |
17300 ksi @Temperature 1800 °F |
|
Carlson C 825 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion st.. |
|||
Modulus of Elasticity | 119 GPa | 17300 ksi | Trans. |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Modulus of Elasticity | 119 GPa | 17300 ksi | Long. |
ATI Wah Chang 425™ Titanium Alloy, Cold Rolled Sheet ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |