Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Pacific Sintered Materials F-241-S Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-15All information provided by Pacific Sintered Metals. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Honeywell Spectra® 900 Fiber Spectra® fiber 900 was the first commercially available extended-chain, high-strength polyethylene fiber and the first in a series of Spectra® fibers. Spectra® fiber has one of the highest .. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Modulus of Elasticity | 117 GPa @Temperature 1000 °C |
17000 ksi @Temperature 1830 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Schott N-LAK34 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Cadi 150 Copper Alloy A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr.. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Cadi 162 Copper Alloy Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium.. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Cadi 1815 Copper Alloy Zirconium addition to chromium copper improves creep resistance at high operating temperatures and reportedly reduces sticking of electrodes to the work during spot welding of galvanized materials. .. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Cadi 182 Copper Alloy Chromium copper is the primary copper alloy used for resistance spot and seam welding. This alloy achieves good hardness and electrical conductivity through a combination of heat treatment and cold .. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
California Fine Wire Alloy 446 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireInsulatedInformation provided by California Fine Wire. |
|||
Modulus of Elasticity | 117 GPa | 17000 ksi | |
Schmolz + Bickenbach MoldMAX XL® Copper Alloy Description: Brush Wellman’s MoldMAX XL® is a high strength copper mold alloy with good thermal conductivity. The alloy contains no beryllium and is available in sections as large as 12” thick. .. |