Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 113.8 GPa | 16510 ksi | In rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 113.8 GPa | 16510 ksi | In rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 113.8 GPa | 16510 ksi | In rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 113.8 GPa | 16510 ksi | In rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 113.8 GPa | 16510 ksi | In rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 113.8 GPa @Temperature 649 °C |
16510 ksi @Temperature 1200 °F |
|
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13) No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa.. |
|||
Modulus of Elasticity | 113.8 GPa | 16510 ksi | In rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |