Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.100 - 7.00 GPa | 14.5 - 1020 ksi | Average value: 1.54 GPa Grade Count:94 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 0.100 - 0.370 GPa | 14.5 - 53.7 ksi | |
MetaFoam Copper Foam General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional†metal foams. MetaFoam can .. |
|||
Modulus of Elasticity | 0.100 GPa | 14.5 ksi | ASTM D638 |
ITW Plexus Plexusâ„¢ 3940 Methacrylate Adhesive An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.Fast tacking, low pressure sprayable adhesive with long bonding range, .. |
|||
Modulus of Elasticity | 0.100 - 0.370 GPa | 14.5 - 53.7 ksi | |
MetaFoam Copper-Silver Foam General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional†metal foams. MetaFoam can .. |
|||
Modulus of Elasticity | 0.100 GPa | 14.5 ksi | ISO 527-2 |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Modulus of Elasticity | 0.100 - 3.30 GPa | 14.5 - 479 ksi | Average value: 1.75 GPa Grade Count:25 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Modulus of Elasticity | 0.100 - 13.0 GPa | 14.5 - 1890 ksi | Average value: 1.50 GPa Grade Count:209 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |