Polymer Property : Modulus of Elasticity = 126 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.870 GPa
126 ksi
tensile test; ISO 527
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..