Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 75.8 GPa | 11000 ksi | |
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem.. |
|||
Modulus of Elasticity | >= 76.0 GPa @Temperature 200 °C |
>= 11000 ksi @Temperature 392 °F |
Condition T6x (Quench in water at RT) |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Modulus of Elasticity | >= 76.0 GPa @Temperature 200 °C |
>= 11000 ksi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Modulus of Elasticity | 76.0 GPa | 11000 ksi | |
Piezo Kinetics 402 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance .. |
|||
Modulus of Elasticity | 76.0 GPa | 11000 ksi | |
Piezo Kinetics 409E Lead Zirconate Titanate Piezoelectric Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance .. |
|||
Modulus of Elasticity | 76.0 GPa | 11000 ksi | |
Schott LITHOTEC-CAF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 76.0 GPa | 11000 ksi | |
Schott N-PSK53A Glass Information Provided by SCHOTT North America, Inc. |