Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 7.20 - 16.0 GPa @Temperature 60.0 - 150 °C |
1040 - 2320 ksi @Temperature 140 - 302 °F |
Average value: 11.7 GPa Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Modulus of Elasticity | 7.20 GPa | 1040 ksi | ASTM D638 |
Toyobo T-750 Nylon, Painting Grade Key Feature: Glass fiber and mineral reinforced, high heat distortion gradesInformation provided by Toyobo Co., Ltd |
|||
Modulus of Elasticity | 7.20 GPa | 1040 ksi | When curved |
Voloknohim PA-SV30 Glass and Mineral Filled Information provided by Voloknokhim |
|||
Modulus of Elasticity | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Modulus of Elasticity | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Conditioned) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Modulus of Elasticity | 7.20 GPa | 1040 ksi | ISO 527 |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Modulus of Elasticity | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned) Description: 30% glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of high stiffness and dimensional stability such as lamp socket housings, f.. |
|||
Modulus of Elasticity | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
BASF Ultramid® A3HG6 Balance 30% Glass Filled PA 66/610 (Conditioned) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |