Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Material ”S”® 8000 Polyethylene Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® Natural Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® natural has excell.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® plus + FP Polyethylene Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from .. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive This material is electrically conductive and has half the sliding friction coefficient of the Original Material ”S”® enabling voltage to be dissipated at maximum speed with the same maximum frict.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | |
Murtfeldt Original Material ”S”® plus + TLS Polyethylene Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | 1 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Modulus of Elasticity | 0.700 - 13.6 GPa | 102 - 1970 ksi | Average value: 4.94 GPa Grade Count:33 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Modulus of Elasticity | 0.700 - 5.00 GPa | 102 - 725 ksi | Average value: 2.51 GPa Grade Count:195 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | ISO 178 |
Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | ISO 178 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | ISO 178 |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | ISO R527 |
Arkema Group Orgalloy® LE 60 LM Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2 R Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 GPa | 102 ksi | Conditioned; ISO 178 |
Addiplast Addinyl PMD 20143 Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 0.700 - 1.34 GPa | 102 - 195 ksi | Average value: 0.961 GPa Grade Count:20 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |