Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.074980 GPa | 10.875 ksi | |
Humiseal 2A64 Urethane Conformal Coating Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F.. |