Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0110 - 2.07 GPa
1.60 - 300 ksi
Average value: 0.243 GPa Grade Count:12
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Modulus of Elasticity 0.0110 - 0.700 GPa
1.60 - 102 ksi
Average value: 0.0939 GPa Grade Count:21
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Modulus of Elasticity 0.0110 GPa
1.60 ksi
ASTM D412 Method A
Seals Eastern 7265D Fluorocarbon-Elastomer
Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc.
Modulus of Elasticity 0.0110 GPa
1.60 ksi
Molded sample
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u..
Modulus of Elasticity 0.0110 GPa
1.60 ksi
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Modulus of Elasticity 0.0110 GPa
1.60 ksi
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Modulus of Elasticity 0.0110 - 0.413 GPa
1.60 - 59.9 ksi
Average value: 0.179 GPa Grade Count:28
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..
Modulus of Elasticity 0.0110 GPa
1.60 ksi
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..