Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.000290 GPa | 0.0421 ksi | 600% Modulus |
UBE UBEPOL BR150 Synthetic Rubber (Compound) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |