Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0000689 - 3.30 GPa
0.0100 - 479 ksi
Average value: 2.45 GPa Grade Count:19
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..