Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.00 - 9.80 GPa @Temperature 60.0 - 150 °C |
435 - 1420 ksi @Temperature 140 - 302 °F |
Average value: 5.86 GPa Grade Count:2 |