Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.225 - 7.80 GPa | 32.6 - 1130 ksi | Average value: 2.37 GPa Grade Count:101 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 1.70 - 7.80 GPa @Temperature 60.0 - 150 °C |
247 - 1130 ksi @Temperature 140 - 302 °F |
Average value: 4.22 GPa Grade Count:6 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 4.30 - 7.80 GPa @Temperature 60.0 - 120 °C |
624 - 1130 ksi @Temperature 140 - 248 °F |
Average value: 6.02 GPa Grade Count:2 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Modulus of Elasticity | 2.70 - 7.80 GPa @Temperature 60.0 - 150 °C |
392 - 1130 ksi @Temperature 140 - 302 °F |
Average value: 4.75 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |