Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.350 - 7.20 GPa @Temperature 60.0 - 150 °C |
50.8 - 1040 ksi @Temperature 140 - 302 °F |
Average value: 2.13 GPa Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Modulus of Elasticity | 2.10 - 7.20 GPa @Temperature 60.0 - 150 °C |
305 - 1040 ksi @Temperature 140 - 302 °F |
Average value: 4.28 GPa Grade Count:3 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Modulus of Elasticity | 2.10 - 7.20 GPa @Temperature 60.0 - 150 °C |
305 - 1040 ksi @Temperature 140 - 302 °F |
Average value: 4.04 GPa Grade Count:2 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Modulus of Elasticity | 2.20 - 7.20 GPa | 319 - 1040 ksi | Average value: 4.32 GPa Grade Count:20 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |