Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.00 - 7.00 GPa | 725 - 1020 ksi | Compression; ISO 527 |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Modulus of Elasticity | 5.00 - 7.00 GPa | 725 - 1020 ksi | Compression; ISO 527 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Modulus of Elasticity | 5.00 - 7.00 GPa | 725 - 1020 ksi | Injection; ISO 527 |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
Modulus of Elasticity | 5.00 - 7.00 GPa | 725 - 1020 ksi | Injection; ISO 178 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Modulus of Elasticity | 5.00 - 7.00 GPa | 725 - 1020 ksi | Injection; ISO 527 |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Modulus of Elasticity | 5.00 - 7.00 GPa | 725 - 1020 ksi | Injection; ISO 527 |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Modulus of Elasticity | 5.00 - 7.00 GPa | 725 - 1020 ksi | Compression; ISO 527 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Modulus of Elasticity | 2.90 - 7.00 GPa | 420 - 1020 ksi | Average value: 4.13 GPa Grade Count:21 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Modulus of Elasticity | 0.100 - 7.00 GPa | 14.5 - 1020 ksi | Average value: 1.54 GPa Grade Count:94 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 3.10 - 7.00 GPa | 450 - 1020 ksi | Average value: 6.21 GPa Grade Count:12 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Modulus of Elasticity | 2.55 - 7.00 GPa | 370 - 1020 ksi | Average value: 5.73 GPa Grade Count:12 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |