Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.68 - 5.40 GPa | 244 - 783 ksi | Average value: 3.00 GPa Grade Count:22 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Modulus of Elasticity | 0.950 - 5.40 GPa | 138 - 783 ksi | Average value: 2.41 GPa Grade Count:147 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |