Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.80 - 5.20 GPa | 551 - 754 ksi | Average value: 4.73 GPa Grade Count:3 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Modulus of Elasticity | 1.83 - 5.20 GPa | 265 - 754 ksi | Average value: 3.45 GPa Grade Count:43 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |