Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 9.65 - 41.7 GPa | 1400 - 6050 ksi | Average value: 18.4 GPa Grade Count:14 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |