Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.00 - 37.2 GPa | 580 - 5400 ksi | Average value: 15.3 GPa Grade Count:47 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |