Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.83 - 33.8 GPa | 700 - 4900 ksi | Average value: 23.6 GPa Grade Count:21 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |