Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 8.27 - 32.0 GPa | 1200 - 4640 ksi | Average value: 13.0 GPa Grade Count:25 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Modulus of Elasticity | 0.500 - 32.0 GPa @Temperature -40.0 - 230 °C |
72.5 - 4640 ksi @Temperature -40.0 - 446 °F |
Average value: 8.06 GPa Grade Count:40 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Modulus of Elasticity | 12.0 - 32.0 GPa @Temperature 60.0 - 150 °C |
1740 - 4640 ksi @Temperature 140 - 302 °F |
Average value: 22.8 GPa Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Modulus of Elasticity | 14.0 - 32.0 GPa @Temperature 150 - 250 °C |
2030 - 4640 ksi @Temperature 302 - 482 °F |
Average value: 23.3 GPa Grade Count:2 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |