Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.40 - 29.0 GPa @Temperature -40.0 - 250 °C |
493 - 4210 ksi @Temperature -40.0 - 482 °F |
Average value: 12.3 GPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Modulus of Elasticity | 3.40 - 29.0 GPa @Thickness 1.60 - 3.17 mm |
493 - 4210 ksi @Thickness 0.0630 - 0.125 in |
Average value: 12.3 GPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Modulus of Elasticity | 4.50 - 29.0 GPa | 653 - 4200 ksi | Average value: 16.5 GPa Grade Count:8 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Modulus of Elasticity | 10.3 - 29.0 GPa | 1490 - 4210 ksi | Average value: 15.2 GPa Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim.. |
|||
Modulus of Elasticity | 1.60 - 29.0 GPa | 232 - 4200 ksi | Average value: 8.94 GPa Grade Count:55 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |