Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.30 - 27.6 GPa | 333 - 4000 ksi | Average value: 13.0 GPa Grade Count:13 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 6.55 - 27.6 GPa | 950 - 4000 ksi | Average value: 16.2 GPa Grade Count:27 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 1.03 - 27.6 GPa | 150 - 4000 ksi | Average value: 9.05 GPa Grade Count:20 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |