Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 11.0 - 23.5 GPa @Temperature 60.0 - 150 °C |
1600 - 3410 ksi @Temperature 140 - 302 °F |
Average value: 17.6 GPa Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |