Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 21.4427 - 21.4427 GPa @Temperature -40.0 - -40.0 °C |
3110.05 - 3110.05 ksi @Temperature -40.0 - -40.0 °F |
Average value: 21.4 GPa Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |