Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 16.0 - 20.0 GPa | 2320 - 2900 ksi | Injection; ISO 527 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Modulus of Elasticity | 5.86 - 20.0 GPa | 850 - 2900 ksi | Average value: 11.6 GPa Grade Count:36 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Modulus of Elasticity | 4.10 - 20.0 GPa | 595 - 2900 ksi | Average value: 14.3 GPa Grade Count:24 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |