Polymer Property : Modulus of Elasticity = 2.93 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.55 - 2.93 GPa

@Temperature 22.8 °C
370 - 425 ksi

@Temperature 73.0 °F
Ensinger TECAST VEKTON™ 6PB Nylon 6 (PA6)
TECAST VEKTON™ 6PB cushion pads are used to dampen the shock load on the anvil of a pile hammer. Specially formulated from an impact-modified type 6 nylon, they combine the excellent strength of n..