Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.30 - 2.41 GPa | 334 - 350 ksi | Average value: 2.38 GPa Grade Count:6 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 1.80 - 2.41 GPa | 261 - 350 ksi | Average value: 2.09 GPa Grade Count:5 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |