Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.70 - 2.00 GPa | 247 - 290 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_7230 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Modulus of Elasticity | 1.40 - 2.00 GPa | 203 - 290 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8425 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Modulus of Elasticity | 1.40 - 2.00 GPa | 203 - 290 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Modulus of Elasticity | 0.580 - 2.00 GPa @Temperature 60.0 - 150 °C |
84.1 - 290 ksi @Temperature 140 - 302 °F |
Average value: 1.10 GPa Grade Count:1 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Modulus of Elasticity | 0.650 - 2.00 GPa @Temperature 60.0 - 150 °C |
94.3 - 290 ksi @Temperature 140 - 302 °F |
Average value: 1.15 GPa Grade Count:1 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Modulus of Elasticity | 1.70 - 2.00 GPa | 247 - 290 ksi | |
Biomer P226 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |