Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.193 - 17.1 GPa @Temperature -40.0 - 150 °C |
318.1 - 2480 ksi @Temperature -40.0 - 302 °F |
Average value: 8.31 GPa Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |