Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 10.3 - 15.2 GPa | 1500 - 2200 ksi | Average value: 13.0 GPa Grade Count:6 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Modulus of Elasticity | 2.75 - 15.2 GPa | 399 - 2200 ksi | Average value: 8.65 GPa Grade Count:31 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Modulus of Elasticity | 2.76 - 15.2 GPa | 400 - 2200 ksi | Average value: 6.95 GPa Grade Count:59 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Modulus of Elasticity | 3.10 - 15.2 GPa | 450 - 2200 ksi | Average value: 5.35 GPa Grade Count:33 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |