Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.30 - 140 GPa @Temperature -55.0 - 177 °C |
769 - 20300 ksi @Temperature -67.0 - 351 °F |
Average value: 86.9 GPa Grade Count:18 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 120 - 140 GPa | 17400 - 20300 ksi | Youngs Modulus |
MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |