Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.700 - 13.6 GPa | 102 - 1970 ksi | Average value: 4.94 GPa Grade Count:33 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |