Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.96 - 11.7 GPa | 430 - 1700 ksi | Average value: 6.71 GPa Grade Count:14 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Modulus of Elasticity | 3.45 - 11.7 GPa | 500 - 1700 ksi | Average value: 7.36 GPa Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Modulus of Elasticity | 3.00 - 11.7 GPa | 435 - 1700 ksi | Average value: 6.79 GPa Grade Count:38 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Modulus of Elasticity | 2.21 - 11.7 GPa | 320 - 1700 ksi | Average value: 6.25 GPa Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 10.3 - 11.7 GPa | 1500 - 1700 ksi | ASTM D638 |
Premix Premi-Glas® 1200H-24 Polyester SMC
(discontinued **) Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni.. |