Modulus of Elasticity 6.60 - 10.9 GPa
957 - 1580 ksi
Average value: 9.31 GPa Grade Count:20
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..