Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.350 - 0.840 GPa | 50.8 - 122 ksi | Average value: 0.648 GPa Grade Count:7 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |