Polymer Property : Modulus of Elasticity = 0.293 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0517 - 0.293 GPa
7.50 - 42.5 ksi
Average value: 0.176 GPa Grade Count:8
Overview of materials for Polybutene
This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..