Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 760 GPa | 110000 ksi | In Tension |
Cytec Thornel® P-100 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.0.32 m/g yield, 0 or 32 tpm t.. |
|||
Modulus of Elasticity | 760 GPa | 110000 ksi | In Tension |
Cytec Thornel® P-100S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction. The fiber surface has been .. |